Nd:YAG 的双折射讨论?

3.4k 3
发表于 2009-5-20 15:02:16|四川 | 查看全部 阅读模式
请教高手!
We also need to ensure the finished crystals are non-birefringent. Birefringence is often induced during growth, processing, or mounting the crystals. Can you comment on your tests for bi-refringence and also whether you have experience with cuboid or cylindrically cut crystals and which are more likely to exhibit birefringence?

---------------------------------------------------
Nd:YAG、 Nd、Ce:YAG, Er:YAG , Yb:YAG , Cr4+:YAG,釹玻璃,铒玻璃,KTP, LBO, KD*P, Nd:YVO4, sapphire, X/K-lamp.
聚光腔、雪崩管、偏振片、1064/1570/2940系列镜片、冷却液
成都新源汇博光电科技有限公司
电话: 028-66873008
手机: 13320993651
传真: 028-84191951
MSN: zjjdj@hotmail.com
邮件: jianjunzhang@vip.sina.com
http:www.yagcrystal.com

地址: 成都锦江区锦华路一段8号万达广场11B1901
-------------------------------------------

回复|共 3 个

kaka Lv.14 发表于 2009-5-20 15:19:51|北京 | 查看全部
没测试过哦,方条和圆棒散热好就行
Daniel-Yuee Lv.10 发表于 2009-5-20 16:06:51|浙江 | 查看全部
理论上说YAG好像不会有双折射的吧?
forbbs Lv.7 发表于 2009-5-23 08:46:56|湖南 | 查看全部
前一阵子有人讨论过,和切割角以及应力有关,比较复杂吧

回复

您需要登录后才可以回帖 登录 | 注册

本版积分规则

投诉/建议联系

admin@discuz.vip

未经授权禁止转载,复制和建立镜像,
如有违反,追究法律责任
  • 关注公众号
  • 添加微信客服
Copyright © 2026 光电工程师社区 版权所有 All Rights Reserved. Powered by Discuz! X5.0 Licensed 鄂ICP备17021725号-1
关灯 在本版发帖
扫一扫添加微信客服
返回顶部
快速回复 返回顶部 返回列表